PUSEN MELAMINE CHIPBOARD/PARTICLE BOARD
| Product Name | Melamine Particle Board |
| Other names | Melamine faced/coated/laminated/overlay/ finish/surface/Veneered Particle board、Chipboard、Flakeboard or Engineered wood board、Pressed wood panel、Wood-based panel |
| Density Class | 650-680 kg/m³ (standard), 680-720 kg/m³ (high density), >720 kg/m³ (enhanced)(It depends on the type of core board, Hot Pressing Process,and other factors.) |
| Surface Effect Type | Matt/Super Matt/Soft Light/High Gloss/Mirror/Granular/Embossed/Hand-scraped/Rain Thread/Linen /Leather /Brushed/Skin Touch/Anti-fingerprint/Wave/3D Texture/Synchronized Embossed(EIR) |
| Surface Color & Texture | Stone,Cement Texture,Fabric,Leather Texture,Solid Colors (White, Grey, Black,Brown,Blue,Pink Etc.), Wood Grains (Oak, Walnut,Maple,Ash,Cherry,Beech,Teak,Mahogany Etc.), Fancy Patterned Designs,Provide A Color Chart Link,Color Matching Service Is Also Available. |
| Melamine Paper GSM | 80-120 g/m² |
| Core Grade | Standard Grade, Moisture Resistant (HMR) -Green or Black Core, Fire Retardant (FR)-Red Core, Termite Resistant |
| Size | Commonly used: 1220x2440mm (4’x8′),Others: 1200x2400mm (3.9’x7.9′), 1200 x 3600mm (3.9’x11.8′), 1220×2745 mm (4’x9′), 1220x2745mm (4’x10′), 1525 mm x 2440 mm (5’x8′),1525 mm x 3050 mm (5’x10′), 1800 x 3600 mm (5.9’x11.8′), 1830x2440mm (6’x8′), 1830x2745mm (6’x9′), 2135x3050mm(7’x10′),2440x3660mm(8’x10′),Upon To Request |
| Thickness | 8mm-45mm, regular sizes 8 (5/16″), 9 (3/8″), 11 (7/16″), 12 (15/32″), 15 (19/32″), 16 (5/8″), 18 (11/16″),20 (25/32″), 21 (13/16″), 25 (1″), 30 (1-3/16″) 32 ( 5/4″) mm/inch, customizable upon request |
| Core | Poplar, Combi, Pine, Eucalyptus/Hardwood Wood Particles/Chips |
| Production Line Type | Multi-Opening Press Line(Sufoma)/Continuous Flat Press Line(Dieffenbacher) |
| Glue | E0 Glue,E1 Glue,E2 Glue,CARB P2 Glue,MDI(Methylene Diphenyl Diisocyanate) Glue |
| Moisture Content | 4 – 12% |
| Thickness Tolerance | ±0.3mm, ±0.5mm |
| Internal Bond Strength – IB | ≥0.55 Mpa, ≥0.65 Mpa |
| Modulus of Rupture – MOR | 18 – 40 N/mm² or higher |
| Modulus of Elasticity – MOE | 2300 – 3500 MPa or higher |
| Abrasion Resistance | AC2 (>250 rpm), AC3 (>400 rpm), AC4 (>600 rpm) (Refer to EN 438 standard) |
| Thickness Swelling after 24h | Standard Board ≤ 12%, Moisture Resistant Board (MR Chipboard) ≤ 8% |
| Screw Holding Strength – Face and Edge | Face Screw Holding > 1200 N Edge Screw Holding > 700 N |
| Surface Bonding Strength | 1.0 – 1.5 N/mm² or higher |
| MOQ | 42CBM/40’GP.50CBM/40’HQ |
| Packing | Inner Packing:0.2mm Thickness Plastic Bag,Outer Packing:Pallet With Carton And Strapped With Steel Tape |
| Delivery | Within 20 days After Confirm The Order |
| DaysPayment | TT,L/C,DP,MONEYGRAM,WESTERN UNION,PAYPAL |
| Usage | Furniture manufacturing (wardrobes, cabinets, desks, bookshelves, TV cabinets), interior decoration (walls, partitions, ceilings, background walls), kitchen and bathroom moisture-proof decoration, display racks and exhibition booths, commercial space decoration, and handicraft and DIY furniture production |
| Capacity | 10000CBM PER MONTH |
| Standard Compliance & Certifications | EN 310, EN 622-5, EN 14322, JIS A 5905, ASTM E1333, ISO 9001, ISO 14001, FSC, PEFC, CARB, CE Mark, BIS etc. |
How PUSEN Controls the Quality of Melamine Chipboard
At PUSEN, we implement strict quality control throughout the entire production process to ensure every Melamine Chipboard panel delivers stable structure, smooth surface, and consistent decorative performance.
1. Strict Chipboard Core Selection
We carefully select high-quality particle boards with uniform density and strong internal bonding. Each board is inspected for:
Density consistency
Particle size distribution
Internal voids or weak areas
Only stable-grade chipboard is used.
2. Moisture Content Control
All chipboard cores are conditioned under controlled humidity environments. Moisture is strictly controlled to prevent:
Swelling
Warping
Surface bubbling after lamination
3. High-Quality Melamine Paper Selection
We use premium melamine decorative paper with stable color and texture. Each batch is checked for:
Color consistency
Pattern alignment
Surface defect control (scratches, stains, fading)
4. Advanced Hot Press Lamination Process
Melamine paper is laminated onto chipboard under precise hot press conditions. We strictly control:
Temperature
Pressure
Pressing time
This ensures strong bonding and smooth, bubble-free surface.
5. Surface Flatness & Finishing Control
After pressing, each board is checked for:
Surface smoothness
Flatness consistency
No bubbling or delamination
No pressing marks or defects
6. Edge & Machining Quality Control
We ensure good processing performance by checking:
Clean cutting edges
No chipping or crumbling
Stable internal structure after CNC cutting
7. Final Quality Inspection Before Shipment
Every sheet undergoes strict final QC, including:
Thickness tolerance
Surface appearance
Color consistency
Structural integrity
Moisture stability
Only fully qualified products are approved for export.
PUSEN Commitment